Material Notes:
Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/13.5 ratio. Pot life: 500 g, 36 min. at 25°C (77°F). Exothermic Peak 265°C (510°F). Hardens in 2-24 hours at RT (faster with heat). Full cure in 1-5 weeks at RT or 1-4 hrs at 80-120°C (175-250°F).
Physical Properties Metric English Comments
Viscosity Measurement 400
400
Mechanical Properties Metric English Comments
Hardness, Rockwell M 96
96
Tensile Strength, Ultimate 73.84 MPa
10710 psi
Elongation at Break 7.5 %
7.5 %
Flexural Yield Strength 81.56 MPa
11830 psi
Flexural Modulus 2.79 GPa
405 ksi
Compressive Yield Strength 98.25 MPa
14250 psi
Compressive Modulus 2.10 GPa
305 ksi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 84.0 °C
183 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity 1.19e+16 ohm-cm
1.19e+16 ohm-cm
Surface Resistance >= 1.19e+16 ohm
>= 1.19e+16 ohm
Dielectric Constant 3.31

@Frequency 1e+6 Hz
3.31

@Frequency 1e+6 Hz
3.77

@Frequency 1000 Hz
3.77

@Frequency 1000 Hz
3.84

@Frequency 60 Hz
3.84

@Frequency 60 Hz
Dissipation Factor 0.0079

@Frequency 60 Hz
0.0079

@Frequency 60 Hz
0.017

@Frequency 1000 Hz
0.017

@Frequency 1000 Hz
0.028

@Frequency 1e+6 Hz
0.028

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Pot Life 36 min
36 min
500 g
Descriptive Properties Value Comments
Exotherm 265°C
Peak
Users viewing this material also viewed the following: