Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | <= 0.30 ohm | <= 0.30 ohm | |
P & P Technology MW Series Conductive Fabric Material: Nylon/PET/Nickel/Copper fabric Self Adhesive Tape: Conductive double sided acrylic carrier and adhesiveInformation provided by P & P Technology |