Polymer Property : Surface Resistance = 0.0060 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance <= 0.0060 ohm
<= 0.0060 ohm
Initial Taber Abrasion (SR); CHO-TP-57
Parker Chomerics CHO-FOIL CCH Shielding Tape
Conductive Adhesive Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or ti..