Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | <= 0.0060 ohm | <= 0.0060 ohm | Initial Taber Abrasion (SR); CHO-TP-57 |
Parker Chomerics CHO-FOIL CCH Shielding Tape Conductive Adhesive Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or ti.. |