Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 8000 V @Thickness 1.57 mm |
8000 V @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S/S |
Industrial Laminates/Norplex NP613 Paper Base Laminate Description: NP613 is constructed from electrical grade of kraft paper and a specially modified epoxy resin system. It is designed to be used in tap changers, coil support plates and terminal panels.. |
|||
Dielectric Breakdown | >= 8000 V @Temperature 90.0 °C, Time 20.0 sec |
>= 8000 V @Temperature 194 °F, Time 0.00556 hour |
Step -by-step test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe PF CC 23 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical and electrical applications. Very coarse weave ( |
|||
Dielectric Breakdown | >= 8000 V @Temperature 90.0 °C, Time 60.0 sec |
>= 8000 V @Temperature 194 °F, Time 0.0167 hour |
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe PF CC 23 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical and electrical applications. Very coarse weave ( |