Polymer Property : Dielectric Breakdown = 8000 V Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Breakdown 8000 V

@Thickness 1.57 mm
8000 V

@Thickness 0.0620 in
Cond D-48/50; ASTM D229 S/S
Industrial Laminates/Norplex NP613 Paper Base Laminate
Description: NP613 is constructed from electrical grade of kraft paper and a specially modified epoxy resin system. It is designed to be used in tap changers, coil support plates and terminal panels..
Dielectric Breakdown >= 8000 V

@Temperature 90.0 °C,
Time 20.0 sec
>= 8000 V

@Temperature 194 °F,
Time 0.00556 hour
Step -by-step test, In oil, parallel to laminations; IEC 1212-2 5.1
Hippe PF CC 23 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Rolled Tube
Used in mechanical and electrical applications. Very coarse weave (
Dielectric Breakdown >= 8000 V

@Temperature 90.0 °C,
Time 60.0 sec
>= 8000 V

@Temperature 194 °F,
Time 0.0167 hour
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1
Hippe PF CC 23 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Rolled Tube
Used in mechanical and electrical applications. Very coarse weave (