Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 20000 V @Thickness 0.430 mm |
20000 V @Thickness 0.0169 in |
ASTM D149 |
Mapal Plastics Maplon CFA-HK Polypropylene Sheet Applications: For use with electrical insulation products. For use when flame retardant and static dissipative properties are required. |
|||
Dielectric Breakdown | 20000 V @Thickness 1.57 mm |
20000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP329 Cotton Fabric Description: Bleached linen with melamine resin system. Provides better arc resistance than NP320E. Also, resistant to ammonia based refrigerants. Hard, durable material should be heated to punch, .. |
|||
Dielectric Breakdown | >= 20000 V @Temperature 90.0 °C, Time 20.0 sec |
>= 20000 V @Temperature 194 °F, Time 0.00556 hour |
Step-by-step test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe SI MP 21 Mica Paper Reinforced Silicone Resin - Round, Rolled Tube Used in mechanical, electrical and electronic applications. Good stability of electrical properties at elevated temperatures.Information provided by Hippe. |
|||
Dielectric Breakdown | >= 20000 V @Temperature 90.0 °C, Time 60.0 sec |
>= 20000 V @Temperature 194 °F, Time 0.0167 hour |
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe SI MP 21 Mica Paper Reinforced Silicone Resin - Round, Rolled Tube Used in mechanical, electrical and electronic applications. Good stability of electrical properties at elevated temperatures.Information provided by Hippe. |
|||
Dielectric Breakdown | 20000 V @Thickness 1.57 mm |
20000 V @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S/S |
Industrial Laminates/Norplex NP321 Cotton Fabric
(discontinued **) Description: NP321 consists of a fine weave cotton fabric (linen) impregnated with a phenolic resin binder. Applications include vanes for air and liquid pumps, and compressors. NP321 remains very f.. |