Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 17500 V @Thickness 0.250 mm |
17500 V @Thickness 0.00984 in |
1/4 inch electrode; ASTM D149 |
Victrex® APTIV® 1000-050 Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline APTIV PEEK 1000 series films are the unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTI.. |
|||
Dielectric Breakdown | 17500 V @Thickness 0.178 mm |
17500 V @Thickness 0.00700 in |
ASTM D149 |
DuPont Teijin Films Melinex® ST507 Polyester Film Melinex® ST507 is a slightly hazy, heat stabilized, polyester film. It has good handling characteristics and is recommended for silver circuitry applications, particularly where an adhesion topcoat.. |