Polymer Property : Electrical Resistivity = 9000 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity <= 9000 ohm-cm
<= 9000 ohm-cm
Shakespeare Sanstat® CN125 .52mm Nylon 66 Monofilament
Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.Information provided by ..
Electrical Resistivity 9000 ohm-cm
9000 ohm-cm
Average
Shakespeare Sanstat® CN125 .36mm Nylon 66 Monofilament
Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.Information provided by ..
Electrical Resistivity 9000 ohm-cm
9000 ohm-cm
St. Cloud Natural Zeolite (Clinoptilolite)
Natural zeolites are microporous volcanic minerals with sieving and cation exchange properties for use in agriculture, environmental and industrial applications. Features such as a vary large inter..