Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+10 - 9.70e+15 ohm-cm | 1.00e+10 - 9.70e+15 ohm-cm | Average value: 6.90e+14 ohm-cm Grade Count:32 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |