Polymer Property : Electrical Resistivity = 9.05e+12 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 9.05e+12 ohm-cm
9.05e+12 ohm-cm
AGY ZenTron® S-2 Generic S-Glass Fiber
S-2 glass and S-glass have the same composition. S-glass is no longer made by AGY, but used to have a reactive epoxy size. Various silanes and starch oil are used as binders. Acid resistant. Mod..