Electrical Properties Metric English Comments
Electrical Resistivity 7.945e+15 ohm-cm
7.945e+15 ohm-cm
ASTM D257
Plenco 51130 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 51130 is an engineering grade UL flame rated glass reinforced recycled polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in black only.Inform..