Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 51130 PET, Pellet, Injection Molded, Black  (discontinued **)

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Recycled, Glass Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 51130 PET, Pellet, Injection Molded, Black  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 51130 is an engineering grade UL flame rated glass reinforced recycled polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in black only.Information supplied by PlencoPlenco discontinued their PET product line in 2005.
Physical Properties Metric English Comments
Density 1.72 g/cc
0.0621 lb/in³
ASTM D792
Water Absorption 0.050 %
0.050 %
ASTM D570
Linear Mold Shrinkage 0.0011 cm/cm
0.0011 in/in
ATM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 19
19
ASTM D785
Tensile Strength, Ultimate 133.4 MPa
19350 psi
ASTM D638
Elongation at Break 1.51 %
1.51 %
ASTM D638
Tensile Modulus 10.79 GPa
1565 ksi
ASTM D638
Flexural Yield Strength 199.7 MPa
28960 psi
ASTM D790
Flexural Modulus 10.58 GPa
1535 ksi
ASTM D790
Compressive Yield Strength 161.5 MPa
23420 psi
ASTM D695
Izod Impact, Notched 0.620 J/cm
1.16 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 221 °C
430 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.47 mm
V-0

@Thickness 0.0579 in
Oxygen Index 31.5 %
31.5 %
ASTM D2863
Electrical Properties Metric English Comments
Electrical Resistivity 7.945e+15 ohm-cm
7.945e+15 ohm-cm
ASTM D257
Dielectric Constant 3.2

@Frequency 1e+6 Hz
3.2

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm
381 kV/in
Short Time; ASTM D149
Dissipation Factor 0.011

@Frequency 1e+6 Hz
0.011

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 70 sec
70 sec
ASTM D495
Comparative Tracking Index 200 V
200 V
ASTM D3638
Copyright © lookpolymers.com All Rights Reserved