Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 7.90e+14 ohm-cm | 7.90e+14 ohm-cm | ASTM D257 |
Ashley Polymers Ashlene® 831 Nylon 6 General purpose extrusion grade for wire jacketing, tubing, rods, slabs and centrifugal casting. ASHLENE 831 meets FDA requirements and is therefore also suitable for film extrusion and co-extrusio.. |