Ashley Polymers Ashlene® 831 Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 831 Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose extrusion grade for wire jacketing, tubing, rods, slabs and centrifugal casting. ASHLENE 831 meets FDA requirements and is therefore also suitable for film extrusion and co-extrusion applications.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Water Absorption 1.9 %
1.9 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
ASTM D785
Tensile Strength, Ultimate 100 MPa
14500 psi
ATSM D638
Elongation at Yield 70 %
70 %
ASTM D638
Flexural Modulus 2.80 GPa
406 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
0.210 J/cm

@Temperature -40.0 °C
0.393 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
ASTM D3418
Electrical Properties Metric English Comments
Electrical Resistivity 7.90e+14 ohm-cm
7.90e+14 ohm-cm
ASTM D257
Dielectric Constant 4.7

@Frequency 1e+6 Hz
4.7

@Frequency 1e+6 Hz
ASTM D150