Polymer Property : Electrical Resistivity = 4.90e+10 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 4.90e+10 ohm-cm
4.90e+10 ohm-cm
Covestro Desmopan® 487 Thermoplastic Polyurethane
Desmopan 487 is a TPU on the basis of a special ester.Applications: Seals, gear wheels, shoe heels, engineering components in the automotive sector.Information provided by Bayer.As of 1 September 20..
Electrical Resistivity 4.90e+10 - 5.00e+14 ohm-cm
4.90e+10 - 5.00e+14 ohm-cm
Average value: 6.77e+13 ohm-cm Grade Count:8
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a..