Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 4.86e+15 ohm-cm | 4.86e+15 ohm-cm | |
Abatron AboCast 50-6/AboCure 50-1 Epoxy Data provided by the manufacturer, Abatron, Inc. Motor oil viscosity, light amber color. Peak exothermic temperature is 160°C (320°F). Shelf life is 12+ months. |