Electrical Resistivity 4.36e+11 ohm-cm
4.36e+11 ohm-cm
ASTM D257
Plenco Valite 424 Novolac Phenolic, Granular, Injection Molded  (discontinued **)
This Valite product has been replaced by Plenco 2424. Data provided by Plenco.VALITE 424 is a black, two stage, general purpose phenolic molding compound. It has a good balance of properties for a ..