Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 4.36e+11 ohm-cm | 4.36e+11 ohm-cm | ASTM D257 |
Plenco Valite 424 Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 2424. Data provided by Plenco.VALITE 424 is a black, two stage, general purpose phenolic molding compound. It has a good balance of properties for a .. |