Polymer Property : Electrical Resistivity = 4.00e+16 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+11 - 4.00e+16 ohm-cm
1.00e+11 - 4.00e+16 ohm-cm
Average value: 1.05e+15 ohm-cm Grade Count:72
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..
Electrical Resistivity 5.00e+14 - 4.00e+16 ohm-cm
5.00e+14 - 4.00e+16 ohm-cm
Average value: 7.72e+15 ohm-cm Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..
Electrical Resistivity 1000 - 4.00e+16 ohm-cm
1000 - 4.00e+16 ohm-cm
Average value: 1.25e+16 ohm-cm Grade Count:37
Overview of materials for Polypropylene with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i..