Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1000 - 1.00e+18 ohm-cm | 1000 - 1.00e+18 ohm-cm | Average value: 2.51e+16 ohm-cm Grade Count:75 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Electrical Resistivity | 1000 - 1.00e+16 ohm-cm | 1000 - 1.00e+16 ohm-cm | Average value: 2.18e+15 ohm-cm Grade Count:12 |
Overview of materials for Polyphthalamide (PPA), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Electrical Resistivity | 1000 - 1.00e+18 ohm-cm | 1000 - 1.00e+18 ohm-cm | Average value: 1.25e+17 ohm-cm Grade Count:110 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Electrical Resistivity | 1000 - 1.00e+17 ohm-cm | 1000 - 1.00e+17 ohm-cm | Average value: 3.33e+16 ohm-cm Grade Count:6 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi.. |
|||
Electrical Resistivity | 1000 - 10000 ohm-cm | 1000 - 10000 ohm-cm | Average value: 2500 ohm-cm Grade Count:6 |
Overview of materials for PPE/PPO + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Electrical Resistivity | 1000 - 1.00e+6 ohm-cm | 1000 - 1.00e+6 ohm-cm | ASTM D257 |
PolyOne Stat-Tech™ AS-15CP/000 ABS - 15% Carbon Powder
(discontinued **) Data provided by PolyOne. |
|||
Electrical Resistivity | 1000 - 1.00e+16 ohm-cm | 1000 - 1.00e+16 ohm-cm | Average value: 6.64e+15 ohm-cm Grade Count:22 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Electrical Resistivity | 1000 - 1.00e+16 ohm-cm | 1000 - 1.00e+16 ohm-cm | Average value: 5.11e+15 ohm-cm Grade Count:11 |
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu.. |
|||
Electrical Resistivity | 1000 - 1.00e+15 ohm-cm | 1000 - 1.00e+15 ohm-cm | Average value: 1.99e+14 ohm-cm Grade Count:22 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Electrical Resistivity | 1000 - 15000 ohm-cm | 1000 - 15000 ohm-cm | |
Heraeus Cleviosâ„¢ P Jet (OLED) Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P Jet (OLED) is an antistatic material based o.. |
|||
Electrical Resistivity | 1000 - 10000 ohm-cm | 1000 - 10000 ohm-cm | ASTM C611 |
Techmer ES Electrafil® J-50/CF/10 Polycarbonate, 10% Carbon Fiber Reinforced Carbon Fiber Reinforced |
|||
Electrical Resistivity | 1000 ohm-cm | 1000 ohm-cm | Specific Resistance |
UBE Tyranno Grade D Ceramic Semi-Conductive Fiber Description: Tyranno Fiber is the continuous ceramic fiber consisting of Si, Ti or Zr,C and O. Advanced composites reinforced by the Tyranno Fiber are expected to play a very important role in the e.. |
|||
Electrical Resistivity | <= 1000 ohm-cm @Temperature 1000 °C |
<= 1000 ohm-cm @Temperature 1830 °F |
ASTM D1829 |
CoorsTek Dura-Z™ MgO Partially Stabilized Zirconia Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | <= 1000 ohm-cm @Temperature 500 °C |
<= 1000 ohm-cm @Temperature 932 °F |
ASTM D1829 |
CoorsTek SC-DSG (SC-35) Graphite Loaded Sintered Silicon Carbide Thermal Shock Delta Tc = 600°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | <= 1000 ohm-cm @Temperature 1000 °C |
<= 1000 ohm-cm @Temperature 1830 °F |
ASTM D1829 |
CoorsTek YZTP Yttria Partially Stabilized Zirconia, Hipped Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | 1000 - 1.00e+16 ohm-cm | 1000 - 1.00e+16 ohm-cm | Average value: 7.38e+15 ohm-cm Grade Count:53 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Electrical Resistivity | 1000 - 1.00e+17 ohm-cm | 1000 - 1.00e+17 ohm-cm | Average value: 3.58e+15 ohm-cm Grade Count:28 |
Overview of materials for Polyether Block Amide (PEBA) This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a.. |
|||
Electrical Resistivity | <= 1000 ohm-cm | <= 1000 ohm-cm | IEC 60093 |
CENTROPLAST CENTROLEN PP LF Polypropylene conductive This material is a low density, easily machined plastic that can be welded and has good surface conductivity. Applications include filter heads and housings, conveyor equipment for flammable liquid.. |
|||
Electrical Resistivity | 1000 - 1.00e+17 ohm-cm | 1000 - 1.00e+17 ohm-cm | Average value: 8.62e+15 ohm-cm Grade Count:26 |
Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |