Electrical Properties Metric English Comments
Electrical Resistivity 1.30e+10 - 4.00e+14 ohm-cm

@Temperature 65.0 - 130 °C
1.30e+10 - 4.00e+14 ohm-cm

@Temperature 149 - 266 °F
Average value: 5.00e+13 ohm-cm Grade Count:8
Overview of materials for Thermoset Polyurethane, Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values ..