Polymer Property : Electrical Resistivity = 3.50e+14 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 - 3.50e+14 ohm-cm
1.00e+14 - 3.50e+14 ohm-cm
Average value: 1.68e+14 ohm-cm Grade Count:11
Overview of materials for Nylon 11, Powder
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Powder". Each property range of values reported is minimum and maximum values of appropriate M..