Polymer Property : Electrical Resistivity = 3.00e+6 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 3.00e+6 ohm-cm

@Temperature 1000 °C
3.00e+6 ohm-cm

@Temperature 1830 °F
ASTM D1829
CoorsTek PlasmaPure™ Alumina (nom. 99.8% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Electrical Resistivity 3.00e+6 - 4.00e+19 ohm-cm
3.00e+6 - 4.00e+19 ohm-cm
Average value: 8.01e+18 ohm-cm Grade Count:5
Overview of materials for Polyimide, Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app..