Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, at 50% RH
(dis AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre.. |
|||
Electrical Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, at 50% RH
(d AMODEL A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent di.. |
|||
Electrical Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Electrical Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Ryton® R-4-230NA Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4-230NA is an advanced 40% fiberglass reinforced polyphenylene sulfide compound which provides reduced flash and improved processability compare.. |
|||
Electrical Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Ryton® R-4-230BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4-230BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound which provides reduced flash and improved processability compared to oth.. |
|||
Electrical Resistivity | 2.00e+15 ohm-cm | 2.00e+15 ohm-cm | |
Momentive Performance Materials TSE3033 Clear General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |