Polymer Property : Electrical Resistivity = 2.00e+10 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 2.00e+10 ohm-cm
2.00e+10 ohm-cm
GBC Grade 85 Alumina
Data provided by the manufacturer, GBC Materials Corporation.
Electrical Resistivity 2.00e+10 ohm-cm

@Temperature 800 °C
2.00e+10 ohm-cm

@Temperature 1470 °F
Saint-Gobain HS Grade Optical Fused Quartz
HS Grade Optical Fused Quartz is a high purity, low [OH] natural fused quartz. It has excellent IR transmission, useful transmission from 260 to 3500 nm, excellent visual quality with low bubbles, ..
Electrical Resistivity 2.00e+10 ohm-cm

@Temperature 800 °C
2.00e+10 ohm-cm

@Temperature 1470 °F
Saint-Gobain Spectrosil® 1000 Optical Fused Quartz
Spectrosil® 1000 grade is used for non-transmissive mirrors and substrates, and other high purity components which do not require specified optical transmission.Spectrosil® is a synthetic fuse..
Electrical Resistivity 2.00e+10 ohm-cm

@Temperature 800 °C
2.00e+10 ohm-cm

@Temperature 1470 °F
Saint-Gobain Spectrosil® 2000 Optical Fused Quartz
Spectrosil® 2000 is a deep UV, fluorescence-free grade.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually chlor..
Electrical Resistivity 2.00e+10 ohm-cm

@Temperature 800 °C
2.00e+10 ohm-cm

@Temperature 1470 °F
Saint-Gobain Spectrosil® 2100 Optical Fused Quartz
Spectrosil® 2100 has improved refractive index homogeneity.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually c..
Electrical Resistivity 2.00e+10 ohm-cm

@Temperature 800 °C
2.00e+10 ohm-cm

@Temperature 1470 °F
Saint-Gobain Spectrosil® 2200 Optical Fused Quartz
Spectrosil® 2200 grade is an excimer laser grade developed for maximum transmission and prolonged life in microlithography and other critical deep UV applications using KrF (248 nm) and ArF (193 ..
Electrical Resistivity 2.00e+10 ohm-cm

@Temperature 800 °C
2.00e+10 ohm-cm

@Temperature 1470 °F
Saint-Gobain Vitreosil® 055 Optical Fused Quartz
Vitreosil® 055 is the highest grade of optical grade fused quartz available from Saint-Gobain Quartz for use in the near UV and visible. It has a useful transmission range from 270 nm in the nea..
Electrical Resistivity 2.00e+10 ohm-cm

@Temperature 800 °C
2.00e+10 ohm-cm

@Temperature 1470 °F
Saint-Gobain Vitreosil® 065 066 Optical Fused Quartz
Vitreosil® 065, for use in the near UV and visible, has a less rigorous bubble specification. It has a useful transmission range from 270 nm in the near UV to 2000 nm in the IR.Vitreosil® opt..
Electrical Resistivity 2.00e+10 ohm-cm

@Temperature 800 °C
2.00e+10 ohm-cm

@Temperature 1470 °F
Saint-Gobain Vitreosil® Clear Fused Quartz Tubing
Electrically fused quartz is recognized for its combination of purity, chemical inertness, physical stability, thermal shock resistance, high electrical resistivity, and high operating temperatures...
Electrical Resistivity 2.00e+10 ohm-cm

@Temperature 800 °C
2.00e+10 ohm-cm

@Temperature 1470 °F
Saint-Gobain Puropsil® B Infrared Grade Low [OH] Optical Fused Quartz
Puropsil® B optical infrared fused quartz is manufactured from naturally occurring quartz crystal using a plasma process to ensure a low OH. It has excellent IR transmission with a useful IR tra..
Electrical Resistivity 2.00e+10 ohm-cm

@Temperature 500 °C
2.00e+10 ohm-cm

@Temperature 932 °F
ASTM D1829
CoorsTek AD-995 Alumina (nom. 99.5% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Electrical Resistivity 2.00e+10 ohm-cm

@Temperature 500 °C
2.00e+10 ohm-cm

@Temperature 932 °F
ASTM D1829
CoorsTek AD-998 Alumina(nom. 99.8% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Electrical Resistivity 2.00e+10 ohm-cm

@Temperature 500 °C
2.00e+10 ohm-cm

@Temperature 932 °F
ASTM D1829
CoorsTek FG-995 Alumina (nom. 98.5% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Electrical Resistivity >= 2.00e+10 ohm-cm

@Temperature 70.0 - 70.0 °C
>= 2.00e+10 ohm-cm

@Temperature 158 - 158 °F
Average value: 1.05e+12 ohm-cm Grade Count:5
Overview of materials for PVC, Molded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb..