Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 2.00e+10 ohm-cm | 2.00e+10 ohm-cm | |
GBC Grade 85 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
Electrical Resistivity | 2.00e+10 ohm-cm @Temperature 800 °C |
2.00e+10 ohm-cm @Temperature 1470 °F |
|
Saint-Gobain HS Grade Optical Fused Quartz HS Grade Optical Fused Quartz is a high purity, low [OH] natural fused quartz. It has excellent IR transmission, useful transmission from 260 to 3500 nm, excellent visual quality with low bubbles, .. |
|||
Electrical Resistivity | 2.00e+10 ohm-cm @Temperature 800 °C |
2.00e+10 ohm-cm @Temperature 1470 °F |
|
Saint-Gobain Spectrosil® 1000 Optical Fused Quartz Spectrosil® 1000 grade is used for non-transmissive mirrors and substrates, and other high purity components which do not require specified optical transmission.Spectrosil® is a synthetic fuse.. |
|||
Electrical Resistivity | 2.00e+10 ohm-cm @Temperature 800 °C |
2.00e+10 ohm-cm @Temperature 1470 °F |
|
Saint-Gobain Spectrosil® 2000 Optical Fused Quartz Spectrosil® 2000 is a deep UV, fluorescence-free grade.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually chlor.. |
|||
Electrical Resistivity | 2.00e+10 ohm-cm @Temperature 800 °C |
2.00e+10 ohm-cm @Temperature 1470 °F |
|
Saint-Gobain Spectrosil® 2100 Optical Fused Quartz Spectrosil® 2100 has improved refractive index homogeneity.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually c.. |
|||
Electrical Resistivity | 2.00e+10 ohm-cm @Temperature 800 °C |
2.00e+10 ohm-cm @Temperature 1470 °F |
|
Saint-Gobain Spectrosil® 2200 Optical Fused Quartz Spectrosil® 2200 grade is an excimer laser grade developed for maximum transmission and prolonged life in microlithography and other critical deep UV applications using KrF (248 nm) and ArF (193 .. |
|||
Electrical Resistivity | 2.00e+10 ohm-cm @Temperature 800 °C |
2.00e+10 ohm-cm @Temperature 1470 °F |
|
Saint-Gobain Vitreosil® 055 Optical Fused Quartz Vitreosil® 055 is the highest grade of optical grade fused quartz available from Saint-Gobain Quartz for use in the near UV and visible. It has a useful transmission range from 270 nm in the nea.. |
|||
Electrical Resistivity | 2.00e+10 ohm-cm @Temperature 800 °C |
2.00e+10 ohm-cm @Temperature 1470 °F |
|
Saint-Gobain Vitreosil® 065 066 Optical Fused Quartz Vitreosil® 065, for use in the near UV and visible, has a less rigorous bubble specification. It has a useful transmission range from 270 nm in the near UV to 2000 nm in the IR.Vitreosil® opt.. |
|||
Electrical Resistivity | 2.00e+10 ohm-cm @Temperature 800 °C |
2.00e+10 ohm-cm @Temperature 1470 °F |
|
Saint-Gobain Vitreosil® Clear Fused Quartz Tubing Electrically fused quartz is recognized for its combination of purity, chemical inertness, physical stability, thermal shock resistance, high electrical resistivity, and high operating temperatures... |
|||
Electrical Resistivity | 2.00e+10 ohm-cm @Temperature 800 °C |
2.00e+10 ohm-cm @Temperature 1470 °F |
|
Saint-Gobain Puropsil® B Infrared Grade Low [OH] Optical Fused Quartz Puropsil® B optical infrared fused quartz is manufactured from naturally occurring quartz crystal using a plasma process to ensure a low OH. It has excellent IR transmission with a useful IR tra.. |
|||
Electrical Resistivity | 2.00e+10 ohm-cm @Temperature 500 °C |
2.00e+10 ohm-cm @Temperature 932 °F |
ASTM D1829 |
CoorsTek AD-995 Alumina (nom. 99.5% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | 2.00e+10 ohm-cm @Temperature 500 °C |
2.00e+10 ohm-cm @Temperature 932 °F |
ASTM D1829 |
CoorsTek AD-998 Alumina(nom. 99.8% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | 2.00e+10 ohm-cm @Temperature 500 °C |
2.00e+10 ohm-cm @Temperature 932 °F |
ASTM D1829 |
CoorsTek FG-995 Alumina (nom. 98.5% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | >= 2.00e+10 ohm-cm @Temperature 70.0 - 70.0 °C |
>= 2.00e+10 ohm-cm @Temperature 158 - 158 °F |
Average value: 1.05e+12 ohm-cm Grade Count:5 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |