Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.22e+16 ohm-cm | 1.22e+16 ohm-cm | |
Abatron AboCast 50-3/AboCure 50-1 Epoxy Data provided by the manufacturer, Abatron, Inc. Honey viscosity, light amber color. Best combination of high strength and versatility for Abatron "VR" Epoxies. Shelf life is 12+ months.Processin.. |
|||
Electrical Resistivity | >= 1.22e+16 ohm-cm | >= 1.22e+16 ohm-cm | |
Abatron AboCast 50-16/AboCure 50-17 Epoxy Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/28 ratio. Pot life: 500 g, 29 min. at 70°C (160°F). Exothermic Peak 242°C (468°F). Cures in 1-2 hrs at .. |
|||
Electrical Resistivity | 1.22e+16 ohm-cm | 1.22e+16 ohm-cm | |
Abatron AboCast 50-3/AboCure 50-17 Epoxy Data provided by the manufacturer, Abatron, Inc. Very low-viscosity; Dark Amber color. Shelf life is 12+ months. |