Polymer Property : Electrical Resistivity = 0.500 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.100 - 0.500 ohm-cm
0.100 - 0.500 ohm-cm
Specific resistance
UBE Tyrannohex® Heat Resistant Composite
Description: Tyrannohex is a fiber assembled ceramic with both toughness like a shell or wood and excellent heat-resistance in air.Very high volume fraction (Vf) of the thin (~ 10m), continuous fibe..