Electrical Properties Metric English Comments
Electrical Resistivity 0.00100 - 0.00300 ohm-cm
0.00100 - 0.00300 ohm-cm
Alliance BCN-11 Bonded (Composite) Magnetic Material
Electrical Resistivity 0.00100 - 0.00300 ohm-cm
0.00100 - 0.00300 ohm-cm
Alliance BCN-13 Bonded (Composite) Magnetic Material
Electrical Resistivity 0.00100 - 0.00300 ohm-cm
0.00100 - 0.00300 ohm-cm
Alliance BCN-10 Bonded (Composite) Magnetic Material
Electrical Resistivity 0.00100 - 0.00300 ohm-cm
0.00100 - 0.00300 ohm-cm
Alliance BCN-12 Bonded (Composite) Magnetic Material
Electrical Resistivity 0.00100 - 0.00300 ohm-cm
0.00100 - 0.00300 ohm-cm
Alliance BCN-14 Bonded (Composite) Magnetic Material
Electrical Resistivity 0.00100 - 0.00300 ohm-cm
0.00100 - 0.00300 ohm-cm
Alliance BCN-15 Bonded (Composite) Magnetic Material
Electrical Resistivity 0.00100 - 0.00300 ohm-cm
0.00100 - 0.00300 ohm-cm
Alliance BCN-17 Bonded (Composite) Magnetic Material