Polymer Property : Electrical Resistivity = 0.00244 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.00244 ohm-cm
0.00244 ohm-cm
Poco Graphite SCF-2 Ion Implant Grade Graphite
An economic alternative to DFP-3-2, this 5-micron material is harder than DFP-3-2 and has high strengths without reduced porosity.