Poco Graphite SCF-2 Ion Implant Grade Graphite

Category Carbon , Graphite
Manufacturer Poco Graphite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Poco Graphite SCF-2 Ion Implant Grade Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
An economic alternative to DFP-3-2, this 5-micron material is harder than DFP-3-2 and has high strengths without reduced porosity.
Physical Properties Metric English Comments
Apparent Bulk Density 1.77 g/cc
0.0639 lb/in³
Particle Size 6.0 µm
6.0 µm
Mechanical Properties Metric English Comments
Hardness, Shore D 91
91
Flexural Strength 93.1 MPa
13500 psi
Compressive Strength 172 MPa
24900 psi
Thermal Properties Metric English Comments
CTE, linear 7.60 µm/m-°C
4.22 µin/in-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00244 ohm-cm
0.00244 ohm-cm
Descriptive Properties Value Comments
Purity 0.999995