Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00193 ohm-cm | 0.00193 ohm-cm | |
Poco Graphite EDM-1 EDM Graphite Applications:Fabricating electrodes with good detail Low wear electrodes High detail roughing electrodesMolds and dies |