Poco Graphite EDM-1 EDM Graphite

Category Carbon , Graphite
Manufacturer Poco Graphite
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Poco Graphite EDM-1 EDM Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:Fabricating electrodes with good detail Low wear electrodes High detail roughing electrodesMolds and dies
Physical Properties Metric English Comments
Particle Size <= 5.0 µm
<= 5.0 µm
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
Flexural Strength 66.9 MPa
9700 psi
Compressive Strength 97.9 MPa
14200 psi
Electrical Properties Metric English Comments
Electrical Resistivity 0.00193 ohm-cm
0.00193 ohm-cm