Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00130 ohm-cm | 0.00130 ohm-cm | |
UCAR Carbon UCAR® ATA Isostatic Molded Graphite Economical grade ATA is the lowest density version of isostatically molded, fine grain grade ATJ family of graphite materials.Typical Applications: ATA is used in general purpose applications where .. |
|||
Electrical Resistivity | 0.00130 ohm-cm | 0.00130 ohm-cm | |
Cytec Thornel® P-25 2K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament strand from a pitch precursor.2000 filaments/strand, 97+% carbon assay, 11 µm filament diameter, 3.1 m/g yield.. |
|||
Electrical Resistivity | 0.00130 ohm-cm | 0.00130 ohm-cm | |
Cytec Thornel® P-25 4K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament strand from a pitch precursor.4000 filaments/strand, 97+% carbon assay, 11 µm filament diameter, 1.4 m/g yield.. |