Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000550 ohm-cm | 0.000550 ohm-cm | |
UCAR Carbon UCAR® SF75 Extruded Graphite Typical uses for extruded grades are in the production of molds and crucibles, heating elements and furnace furniture, liquid metal processing equipment and chemical process equipment.Tabular proper.. |