Material Notes:
Typical uses for extruded grades are in the production of molds and crucibles, heating elements and furnace furniture, liquid metal processing equipment and chemical process equipment.Tabular property data is typical. Information provided by UCAR Carbon Company, a GrafTech International Ltd. company.
Physical Properties Metric English Comments
Density 1.72 g/cc
0.0621 lb/in³
Particle Size <= 750 µm
<= 750 µm
Ash 0.050 %
0.050 %
Mechanical Properties Metric English Comments
Flexural Strength 16.5 MPa
2400 psi
Thermal Properties Metric English Comments
CTE, linear 0.700 µm/m-°C

@Temperature 20.0 - 100 °C
0.389 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 200 W/m-K
1390 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.000550 ohm-cm
0.000550 ohm-cm