Electrical Resistivity 0.0000990 ohm-cm

@Temperature 23.0 °C
0.0000990 ohm-cm

@Temperature 73.4 °F
Special Metals INCOLOY® alloy 028 Austenitic Stainless Steel
INCOLOY® alloy 028 (UNS N08028/W. Nr. 1.4563) is a highly alloyed austenitic stainless steel offering resistance to a variety of corrosive media. By virtue of its contents of chromium and molybd..
Electrical Resistivity 0.0000990 ohm-cm
0.0000990 ohm-cm
ATI Allegheny Ludlum Type 332 Stainless Steel, UNS N08800
Type 332 is a nickel and chromium austenitic stainless steel designed to resist oxidation and carburization at elevated temperatures. The nickel content, 32%, makes the alloy highly resistant both ..
Electrical Resistivity 0.0000990 ohm-cm
0.0000990 ohm-cm
ATI Allegheny Ludlum AL 800AT™ Nickel-Base Alloy, UNS N08811
AL 800AT alloy is nickel-iron-chromium alloys designed to resist oxidation and carburization at elevated temperatures. The nickel content makes the alloy highly resistant both to chloride stress-co..
Electrical Resistivity 0.0000990 ohm-cm
0.0000990 ohm-cm
ATI Allegheny Ludlum AL 800H™ Nickel-Base Alloy, UNS N08810
AL 800H alloy is nickel-iron-chromium alloys designed to resist oxidation and carburization at elevated temperatures. The nickel content makes the alloy highly resistant both to chloride stress-cor..
Electrical Resistivity 0.0000990 ohm-cm
0.0000990 ohm-cm
ATI Allegheny Ludlum AL 800™ Nickel-Base Alloy, UNS N08800
AL 800 alloy is nickel-iron-chromium alloys designed to resist oxidation and carburization at elevated temperatures. The nickel content makes the alloy highly resistant both to chloride stress-corr..