Electrical Properties Metric English Comments
Electrical Resistivity 0.0000989 ohm-cm
0.0000989 ohm-cm
Special Metals INCOLOY® Alloy 800
A nickel-iron-chromium alloy with good strength and excellent resistance to oxidation and carburization in high-temperature atmospheres. It also resists corrosion by many aqueous environments. The..
Electrical Resistivity 0.0000989 ohm-cm
0.0000989 ohm-cm
Special Metals INCOLOY® Alloy 800HT™
A nickel-iron-chromium alloy having the same basic composition as INCOLOY alloy 800 but with significantly higher creep-rupture strength. The higher strength results from close control of the carbo..