Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000780 ohm-cm | 0.0000780 ohm-cm | |
Schmolz + Bickenbach UgiPermâ„¢ 12FM Stainless Steel Bar Description: UgiPermâ„¢ 12FM is a 12% chrome ferritic stainless with improved magnetic properties designed for use in electro-injectors, valves and many other applications. The grade was develope.. |
|||
Electrical Resistivity | 0.0000780 ohm-cm | 0.0000780 ohm-cm | |
AK Steel 309S Austenitic Stainless steel AK Steel 309S provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic w.. |
|||
Electrical Resistivity | 0.0000780 ohm-cm @Temperature 20.0 °C |
0.0000780 ohm-cm @Temperature 68.0 °F |
|
ATI Allegheny Ludlum 310 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Electrical Resistivity | 0.0000780 ohm-cm @Temperature 20.0 °C |
0.0000780 ohm-cm @Temperature 68.0 °F |
|
ATI Allegheny Ludlum 310H Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Electrical Resistivity | 0.0000780 ohm-cm @Temperature 20.0 °C |
0.0000780 ohm-cm @Temperature 68.0 °F |
|
ATI Allegheny Ludlum 310S Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Electrical Resistivity | 0.0000780 ohm-cm @Temperature 20.0 °C |
0.0000780 ohm-cm @Temperature 68.0 °F |
|
ATI Allegheny Ludlum 310Si Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Electrical Resistivity | 0.0000780 ohm-cm | 0.0000780 ohm-cm | |
AK Steel 309 Austenitic Stainless steel AK Steel 309 provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic wh.. |