Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000665 ohm-cm | 0.0000665 ohm-cm | 3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02 |
California Fine Wire Alloy 436 Platinum/Tungsten Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonInsulatedPlatedInformation provided by California Fine Wire. |
|||
Electrical Resistivity | 0.0000665 ohm-cm | 0.0000665 ohm-cm | 3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02 |
California Fine Wire Alloy 436L Precious Metal Alloy All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonInsulatedInformation provided by California Fine Wire. |