Electrical Properties Metric English Comments
Electrical Resistivity 0.00005994 ohm-cm

@Temperature 23.0 °C
0.00005994 ohm-cm

@Temperature 73.4 °F
Crucible Steel 430 Chromium Steel
Crucible 430 is essentially a non-hardenable chromium steel which is adaptable for general purpose corrosion and heat resisting applications. It is prone to slight hardening by heat treatment. This..
Electrical Resistivity 0.00005994 ohm-cm

@Temperature 23.0 °C
0.00005994 ohm-cm

@Temperature 73.4 °F
Crucible Steel 440A Chromium Steel
Crucible 440A is a hardenable chromium steel which is the toughest of the high chromium cutlery grades. This grade is magnetic at all times. Information provided by Crucible Specialty Metals.