Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000590 ohm-cm | 0.0000590 ohm-cm | |
Alpase M-5™ Aluminum Mold Plate Excellent weldabilitySurface Condition - Machined top and bottom to reduce costly handling and machining stepsDimensional Stability - High dimensional stability during and after machiningPolishing -.. |
|||
Electrical Resistivity | 0.0000590 ohm-cm | 0.0000590 ohm-cm | |
Bohler-Uddeholm BÖHLER W360 ISOBLOC® Hot Work Tool Steel BÖHLER W360 ISOBLOC was developed as a tool steel for dies and punches in warm and hot forging. The steel can be used for a variety of applications where hardness and toughness are required. Prope.. |