Polymer Property : Electrical Resistivity = 0.0000550 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000550 ohm-cm
0.0000550 ohm-cm
RT
Outokumpu 4021 Martensitic Stainless Steel
Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat..
Electrical Resistivity 0.0000550 ohm-cm
0.0000550 ohm-cm
Indium Corp. Indalloy 23 Bismuth Solder Alloy
Non-electrical solder for low-ambient temperatureInformation Provided by Indium Corporation
Electrical Resistivity 0.0000550 - 0.0000620 ohm-cm
0.0000550 - 0.0000620 ohm-cm
Goodfellow Nickel Base Magnetic Shielding Alloy - Mu Metal
High Nickel magnetically soft alloy used for magnetic shielding, high quality but low noise audio frequency transformers, ground fault interrupter cores, anti-shoplifting devices, tape recorder head..
Electrical Resistivity 0.0000550 ohm-cm
0.0000550 ohm-cm
AK Steel 420 Martensitic Stainless steel
AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu..
Electrical Resistivity 0.0000550 ohm-cm
0.0000550 ohm-cm
AK Steel 420 ULTRA HONE® Martensitic Stainless steel
AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu..
Electrical Resistivity 0.0000550 ohm-cm
0.0000550 ohm-cm
AK Steel 420HC Martensitic Stainless steel
AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu..
Electrical Resistivity 0.0000550 ohm-cm
0.0000550 ohm-cm
AK Steel 420LC Martensitic Stainless steel
AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu..