Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Electrical Resistivity = 0.0000547 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000547 ohm-cm
0.0000547 ohm-cm
Special Metals MONEL® Alloy 400
A nickel-copper alloy with high strength and excellent corrosion resistance in a range of media including sea water, hydrofluoric acid, sulfuric acid, and alkalis. Used for marine engineering, chem..
Copyright © lookpolymers.com All Rights Reserved