Electrical Resistivity |
0.0000470 - 0.0000530 ohm-cm |
0.0000470 - 0.0000530 ohm-cm |
|
Alliance A-2 Alnico Magnetic Material
|
Electrical Resistivity |
0.0000470 - 0.0000530 ohm-cm |
0.0000470 - 0.0000530 ohm-cm |
|
Alliance A-3 Alnico Magnetic Material
|
Electrical Resistivity |
0.0000470 - 0.0000530 ohm-cm |
0.0000470 - 0.0000530 ohm-cm |
|
Alliance A-5 Alnico Magnetic Material
|
Electrical Resistivity |
0.0000470 - 0.0000530 ohm-cm |
0.0000470 - 0.0000530 ohm-cm |
|
Alliance A-5-7 Alnico Magnetic Material
|
Electrical Resistivity |
0.0000470 - 0.0000530 ohm-cm |
0.0000470 - 0.0000530 ohm-cm |
|
Alliance A-5DG Alnico Magnetic Material
|
Electrical Resistivity |
0.0000470 - 0.0000530 ohm-cm |
0.0000470 - 0.0000530 ohm-cm |
|
Alliance A-6 Alnico Magnetic Material
|
Electrical Resistivity |
0.0000470 - 0.0000530 ohm-cm |
0.0000470 - 0.0000530 ohm-cm |
|
Alliance A-8 Alnico Magnetic Material
|