Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Alliance A-5DG Alnico Magnetic Material

Category Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Cobalt Alloy , Nickel Alloy
Manufacturer Alliance LLC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Alliance A-5DG Alnico Magnetic Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 7.30 g/cc
0.264 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 450 - 700
450 - 700
Thermal Properties Metric English Comments
CTE, linear 11.0 - 13.0 µm/m-°C

@Temperature 20.0 °C
6.11 - 7.22 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Maximum Service Temperature, Air 525 °C
977 °F
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000470 - 0.0000530 ohm-cm
0.0000470 - 0.0000530 ohm-cm
Magnetic Coercive Force, Hc 680 Oe
680 Oe
700 Oe
700 Oe
Intrinsic
Magnetic Remanence, Br 13000 Gauss
13000 Gauss
Magnetic Maximum Energy Product, BH 6.5 MGOe
6.5 MGOe
Curie Temperature 860 °C
1580 °F
Descriptive Properties Value Comments
Reversible Temp Coef., Bd -0.02 %/°C
Reversible Temp Coef., Hd +0.02 %/°C
Temperature Coefficient, Br -0.025 %/°C
(20-100°C)
Temperature Coefficient, Hci +0.01 %/°C
(20-100°C)
Users viewing this material also viewed the following: