Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000420 ohm-cm | 0.0000420 ohm-cm | |
Williams Advanced Alloys C109 Solder Williams extensive offering of Contact Alloys are cast and fabricated to meet the exacting standards of various micro electronics applications. All Williams electrical contact alloys are available i.. |