Polymer Property : Electrical Resistivity = 0.0000420 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000420 ohm-cm
0.0000420 ohm-cm
Williams Advanced Alloys C109 Solder
Williams extensive offering of Contact Alloys are cast and fabricated to meet the exacting standards of various micro electronics applications. All Williams electrical contact alloys are available i..