Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000350 - 0.0000450 ohm-cm | 0.0000350 - 0.0000450 ohm-cm | Parallel (002) |
Mateck Highly Oriented Pyrolytic Graphite Oxidic single crystals. Applications include:Scanning tunneling microscopy-callibration and substratesGraphite monochromatorsx-ray diffractionneutron scattering and diffraction |
|||
Electrical Resistivity | 0.0000350 ohm-cm | 0.0000350 ohm-cm | |
Toho Tenax Besfight® MC Type II (12,000 Filament) Nickel Coated Carbon Fiber Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec.. |
|||
Electrical Resistivity | 0.0000350 ohm-cm | 0.0000350 ohm-cm | |
Toho Tenax Besfight® MC Type II (3000 Filament) Nickel Coated Carbon Fiber Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec.. |
|||
Electrical Resistivity | 0.0000350 ohm-cm | 0.0000350 ohm-cm | |
Toho Tenax Besfight® MC Type II (6000 Filament) Nickel Coated Carbon Fiber Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec.. |
|||
Electrical Resistivity | 0.0000350 - 0.0000450 ohm-cm | 0.0000350 - 0.0000450 ohm-cm | parallel (002) direction |
Momentive Performance Materials HOPG Graphite Monochromator Advanced Ceramics' graphite monochromators are highly oriented forms of high purity pyrolytic graphite which diffract x-rays and neutrons with greater efficiency than any other material. In x-r.. |